101. Pitting
102. Dezincification
103. Expoliation
104. Filiform corrosion
105. Fretting corrosion
106. The corroded member in a corrosion cell is the cathode.
107. 2
108. Stainless steels have tensile moduli greater than those of carbon and alloy steels.
109. Iron, chromium, carbon and nickel
110. 6
111. Casting
112. Metal mold (matching halves)
113. Ductile iron
114.Continuous pultrusion
115. Alkydes
116. 23XX
117. 12XX
118. American Iron and Steel Institute
119. Society of Automotive Engineers
120. American Society for Testing and Materials
121. 16 % to 20 %
122. 600oC to 1100oC
123. Cobalt
124. 0.20
125. 0.15 to 0.30
126. 11 to 14
127. strain harden
128. 11 to 17
129. Casehardening
130. Hardenability
131. 1333o F
132. 770o C
133. Pearlite
134. Alpha iron
135. Nitriding
136. Cassiterite
137. Sphalerite
138. Ilmanite
139. Bauxite
140. copper and zinc
141. copper and tin
142. The alloy group
143. The modifications of the alloy group or impurity limits
144. As fabricated
145. Manganese alloys
146. 50000 lbf/in2
147. less than 0.1 percent
148. 14 %
149. Muntz metal
150. 15 %